Description: Molten metal is injected, under pressure, into hardened steel dies, often water cooled. Dies are opened, and castings are ejected.
Metals: Aluminum, Zinc, Magnesium.
Size Range: Not normally over 2 feet square. Some foundries capable of larger sizes.
Tolerances:
Al and Mg ± .002ʺ/in.
Zinc ± .0015ʺ/in.
Add ± .001ʺ to ± .015ʺ across parting line depending on size
Surface Finish: 32-63RMS
Minimum Draft Requirements:
Al & Mg: 1° to 3°
Zinc: 1/2° to 2°
Normal Minimum Section Thickness:
Al & Mg: .03ʺ Small Parts: .06ʺ Medium Parts
Zinc: .03ʺ Small Parts: .045ʺ Medium Parts
Ordering Quantities: Usually 2,500 and up.
Normal Lead Time: Samples: 12-20 weeks